Warren (Staff)
Warren (Staff)
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Any of our epoxy based adhesives would work well for an aluminium to aluminium bond. Both surfaces should always be keyed first though.
Our
ET500Rigid 5min Epoxy Adhesive
would give a quick and rigid bond.
Our
ET515 Semi Flexible 15min Epoxy Adhesive
takes a little longer to cure and also has a much higher flexural strength where the finished panel is exposed to vibration/shock.
Our
ET538Honeycomb Bonding Epoxy Adhesive
is specially formulated for bonding aluminium to a range of materials (including aluminium) so is probably closest suited for your needs.
Quantity calculations are always hard as it depends on the use. Our adhesives come in 50ml or 400ml packs ie by volume. How much you use would vary between a thin bead and it being spread out. Your initial quantity would suggest to me you are looking at the very least at 1 400ml twin tube to get started with.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
3
adrian.wagstaff@onboardene...
adrian.wagstaff@onboardene...
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 16
Hi
Can you recommend what glue we would be best to use to glue/seal aluminium to aluminium on a boat wheel house roof. Temperature range would be –20 to + 100 DegC.
Could you also help with quantity? We have around 18m of 30mm wide strips to be fixed.
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search