guys , istarted since 3 years doing carbon overlay with polyester resin , and i never used epoxy because we dont have it here , if anyone ants anything to do with polyester resin i surely can help and by the way i started doing infusion too with it and its doing fine.

best regards mhd alghoul mhdghoul@hotmail.com youtube channel :atmospherejo link is http://www.youtube.com/user/atmospherejo?ob=0&feature=results_main