By mhdghoul - 2/1/2012 4:52:24 PM
guys , istarted since 3 years doing carbon overlay with polyester resin , and i never used epoxy because we dont have it here , if anyone ants anything to do with polyester resin i surely can help and by the way i started doing infusion too with it and its doing fine.
|
By mhdghoul - 2/1/2012 6:59:00 PM
if u mean bubles yup i did face that problem but i solved it depending on the quantity of it , i sand it from 120 till 2000 then i clear coat it and it works real fine , some times i used to sand it 2000 again until i level things up next day and re coat it .
also i added a material i dont know its name in english which is sold to make polyester more liquid and this resulted in more tha 70% less bubles sometimes no bubles.
hope this will help
|
|