ANSWER
HOT
Topic Details
Group: Awaiting Activation
Posts: 6,
Visits: 75
I'm going to start attempting to make a interior parts for my Legacy in a few weeks.
I plan on making an outer cf skin, inner fg skin and then bonding them together. The main reason for this is due to the locating pins on the rear of the parts. I can't see a way to include these using just one skin.
My question is, how do I make these pins? The mold should be straight forward enough, but how do I get the fg into the mold to form the part?
Hope that makes sense!
Reply
Like
2
neilb
neilb
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 107,
Visits: 504
i'm guessing the 'pins' are on the rear of the part that locate and hold the part in its correct place. you could take a mould of said locating pins on the rear of the part.
doing a good mould of these pins would help, as it would end up being used to get them in the correct place for bonding. you could go further and make a mould to use as a locater then make another putting wider flanges on it for infusing the parts
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search