Hi - you guys have made it so easy to get hold of a great range of materials.  Thank you.

I build sailing dinghies - mostly wooden ones, but will shortly have a GRP hull with a split side-deck to fix.

It will be a letter-box repair using epoxy and glass cloth (in preference to polyester resin as I really don't like styrene).

Two questions: 

1. Is your gel coat product UV resistant? (Usually I would expect to have to varnish any epoxy finish I use on a dinghy to provide adequate UV protection)

2. When colour matching the existing gel coat, what proportion of pigment can be added to the mix? (Generally I would work on 5% max)

Look forward to hearing from you

Tim Gatti
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
TimG - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search