Jess8bit
Jess8bit
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 133,
Visits: 566
Hello everyone, happy new year ! I whish you many successful composite projects
I wonder what is the best way to build a box in CF, with 4 or 5 sides. The example I have in mind is a typical matches box, both the outer box (where you scratch the match, which is 4-sided) and the inner box (the drawer, where are the matches, which is 5-sided).
What kinds of moulds or plugs to prepare ? How to make perfect 90° angles ? how to bond sides ? Which process (Resin infusion ?) ? Does it require inner reinforcement (like a flat angle bracket) ? Do I need to make the 4-sided in one pass (with one cloth) ?
Thanks for sharing ideas guys
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
How to build a CF box ?
Jess8bit
-
12 Years Ago
hello i have been reading that molds with 90 degree angles can be hard to make the release happen....
brasco
-
12 Years Ago
Thank you Brasco for the idea of bonding 2 L-shaped panels :) and for the interesting links about...
Jess8bit
-
12 Years Ago
hmmm i think one could use wood (a 90 degree joint)and make a section longer than what you need. if...
brasco
-
12 Years Ago
Again, I find it a good idea in making the part twice longer then cut it in half afterwards ! Neat...
Jess8bit
-
12 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search