Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
how to complex print on carbon fiber
how to complex print on carbon fiber
Post Reply
Like
6
how to complex print on carbon fiber
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
ARSOUILLERB26
ARSOUILLERB26
posted 5 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 16,
Visits: 122
Hello mates
I would like to know how to achieve complex printing on carbon fiber.
I would like to do something like this (picture found on a shop so it's possible)
If possible I would like to invoid clear coating because my bodyshop painter had a lot of work clear coating my infused parts (lot of pinholes which forced him to a LOT of layers and of course sanding between each one)
I asked to a serigraphic shop if they can print on carbon fiber and it would be a first try for them so if I can give them some advices, it would be a time/money saver.
Do you know how this printing can be done and if clear coats are necessary, what product can I buy for a carbon fiber specific application? (I saw in the last easy composites video a "phantom clear")
Thank you everybody
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
how to complex print on carbon fiber
ARSOUILLERB26
-
5 Years Ago
Especially with the white, but even without that, i think the only way something like this will ever look good is if it is painted and then clear coated. I For the pin hole story maybe look into wip...
SleepingAwake
-
5 Years Ago
Yeh, definitely something you will want to do with clear over the top. There's other ways, but this is too complex to be reliable. Pinholes are no problem if you've got a decent clear coat. Somethin...
Hanaldo
-
5 Years Ago
Hi and thank you for your replies Lester, what do you mean by: "wipe on fillers"? English is not my main language so I don't see what it is. So I need a polyester top coat instead of the classic 2k...
ARSOUILLERB26
-
5 Years Ago
there are specific products to fill in surface porosity like this one: https://shop1.r-g.de/en/art/954200 Honestly i never worked with a specificly formulated prduct like the one i linked, but...
SleepingAwake
-
5 Years Ago
thanks mate :) I will order it, can't wait to try Just to be sure I understood well, when you use a squegee or a cloth with epoxy resin (infusion resin to be more fluid I suppose) on it before to...
ARSOUILLERB26
-
5 Years Ago
I always used a fast laminating resin rather than a low viscosity infusion resin, altough i doubt it will make too much of a difference. But the higher viscosity and the better polymerization in thin...
SleepingAwake
-
5 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search