+xthanks mate
I will order it, can't wait to try
Just to be sure I understood well, when you use a squegee or a cloth with epoxy resin (infusion resin to be more fluid I suppose) on it before to wipe it.
I tried it with a plastic card (like a credit card) but didn't wipe it off.
It took a looooot of time to cure (3 days in a 40° celcius room) despite I used infusion IN2 resin with FAST remover.
The aspect is actually quite bad and I have to sand it / polish it a lot.
How was the finish for you using your technique?
thanks again
I always used a fast laminating resin rather than a low viscosity infusion resin, altough i doubt it will make too much of a difference. But the higher viscosity and the better polymerization in thin films doesn't harm either. The surface certainly gets a little cloudy, but nothing the usual paint prep wouldn't take care of.