Help/Advice needed about a mould.


Author
Message
Lester Populaire
L
Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
depending on the geometry i would say a PP or PE sheet, or teflon adhesive film. The latter will not result in a mirror finish tho.
Derek Dunning
Derek Dunning
Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)
Group: Forum Members
Posts: 3, Visits: 41
Dentex - 10/7/2021 12:07:38 AM
If I understand correctly, you need something like release film to avoid wax or release agent application before layup.

I am not very experienced but my guess is that you most likely find something like that, because all foils, films etc can wrinkle and mess with finish. But that's just my 2 cents.

Best wishes

Yes I'm looking for some form of film that can be laid into the mould..plan would be to tape it in place.


Dentex
D
Supreme Being (568 reputation)Supreme Being (568 reputation)Supreme Being (568 reputation)Supreme Being (568 reputation)Supreme Being (568 reputation)Supreme Being (568 reputation)Supreme Being (568 reputation)Supreme Being (568 reputation)Supreme Being (568 reputation)
Group: Forum Members
Posts: 42, Visits: 1.4K
If I understand correctly, you need something like release film to avoid wax or release agent application before layup.

I am not very experienced but my guess is that you most likely find something like that, because all foils, films etc can wrinkle and mess with finish. But that's just my 2 cents.

Best wishes
Derek Dunning
Derek Dunning
Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)
Group: Forum Members
Posts: 3, Visits: 41
Greetings to all

I've been playing around with resin infusion and have a very simple mould with a bend that works well.
What I would like to know is what material can I use that's got a high gloss finish that's cheap and either disposable or reusable to lay into the mould
and do the layup on top so I don't need to wax the mould and can peel the material off the mould and fibreglass,

Hope that makes sense....

Thanks in advance

D.
Edited 5 Years Ago by Derek Dunning
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search