By Derek Dunning - 10/6/2021 10:09:30 PM
Greetings to all
I've been playing around with resin infusion and have a very simple mould with a bend that works well. What I would like to know is what material can I use that's got a high gloss finish that's cheap and either disposable or reusable to lay into the mould and do the layup on top so I don't need to wax the mould and can peel the material off the mould and fibreglass,
Hope that makes sense....
Thanks in advance
D.
|
By SleepingAwake - 10/7/2021 10:52:20 AM
depending on the geometry i would say a PP or PE sheet, or teflon adhesive film. The latter will not result in a mirror finish tho.
|
|