Cutting a fabric roll?


Author
Message
Warren (Staff)
Warren (Staff)
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
It cuts like Kevlar albeit not quite as difficult. 

You don't see that many twill format narrow tapes as a plain weave is much easier to manufacture.  Many of the twill formats are woven as a braid, be it flat or tubular.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
The Mould Destroyer
The Mould Destroyer
Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)
Group: Forum Members
Posts: 21, Visits: 332
Fasta - 7/27/2021 8:18:23 AM
You can likely just use a bandsaw although the cut would be a little rough compared to a proper slitting maching.

I imagine a disaster with binding and bandsaw flying around
Or its not like kevlar?

The Mould Destroyer
The Mould Destroyer
Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)
Group: Forum Members
Posts: 21, Visits: 332
Warren (Staff) - 7/27/2021 10:25:06 AM
I can see several options on google?

Ya, but only 300g plain not 200 twill
Anyway, Thanks!

Warren (Staff)
Warren (Staff)
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
I can see several options on google?

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Fasta
Fasta
Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
You can likely just use a bandsaw although the cut would be a little rough compared to a proper slitting maching.




The Mould Destroyer
The Mould Destroyer
Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)
Group: Forum Members
Posts: 21, Visits: 332
Warren (Staff) - 7/26/2021 4:22:32 PM
They are on the market just not a product we ourselves stock. 

Really? I couldn't find any on google
Is it possible for you to share with me (DM) or is it problematic? 

Thanks!

Warren (Staff)
Warren (Staff)
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
They are on the market just not a product we ourselves stock. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
The Mould Destroyer
The Mould Destroyer
Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)
Group: Forum Members
Posts: 21, Visits: 332
width ways, with the roll and everything Smile
I wish there was Diolen tapes, like the kevlar ones... Sad
Warren (Staff)
Warren (Staff)
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Are you talking across the roll or cutting it width ways?  Just use shears normally.  To cut it on the roll would probably be difficult to do without some kind of slitting machine that can roll off the roll, cut and roll back on to another roll.  Its not a service we offer. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
The Mould Destroyer
The Mould Destroyer
Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)
Group: Forum Members
Posts: 21, Visits: 332
What are the ways to cut a roll of fabric? (diolen)
I want to pre cut it to strips so save time

Is there a cheap way to do so?
Also, do Easy composites offer this kind of service?
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search