By The Mould Destroyer - 7/25/2021 1:18:10 PM
What are the ways to cut a roll of fabric? (diolen) I want to pre cut it to strips so save time
Is there a cheap way to do so? Also, do Easy composites offer this kind of service?
|
By Warren (Staff) - 7/28/2021 8:25:59 AM
It cuts like Kevlar albeit not quite as difficult.
You don't see that many twill format narrow tapes as a plain weave is much easier to manufacture. Many of the twill formats are woven as a braid, be it flat or tubular.
|
|