Hi,

I have a table with a span of 188 centimeters (74 inches) that is sagging 1.5 inches (so far)
It is made of MDF clad in linoleum, and thus needs something to make it more sturdy
I am thinking CF strips bonded to the bottom after letting it straighten by laying it on the back

Does anybody have tips/tricks, and which dimensions would be necessary.