Ryan Wise
Ryan Wise
posted 5 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 1
I'm wondering what would be good things to add to resin to make it tougher. Something like JB Weld, but using my existing bisphenol based epoxy, bought in bulk?
Reply
Like
13
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Additives for a tougher resin
Ryan Wise
-
5 Years Ago
You sort of have to keep in mind that different epoxies will have different base properties, it isn't necessarily possible to modify any old epoxy and make it perform like a toughened structural...
Hanaldo
-
5 Years Ago
Just remember that some additives will influence the colour quite a lot. eg fumed silica in any quantity turns the mix opaque white. Milled carbon turns it charcoal black. Glass in larger quantities....
Warren (Staff)
-
5 Years Ago
Post Reply
Like
13
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search