By Ryan Wise - 1/5/2021 8:06:49 PM
I'm wondering what would be good things to add to resin to make it tougher. Something like JB Weld, but using my existing bisphenol based epoxy, bought in bulk?
|
By Warren (Staff) - 1/7/2021 12:14:32 PM
Just remember that some additives will influence the colour quite a lot. eg fumed silica in any quantity turns the mix opaque white. Milled carbon turns it charcoal black. Glass in larger quantities will turn it a bit of a semi-translucent murky grey colour.
|
|