I've got a few patches of fibre print through on a piece I've just finished. i am not too worried about the visual finish and am clear coating it anyway, but I just wanted to check if this was going to compromise the part in any way, i.e. structurally or longevity, or if it is purely an aesthetic issue?

Would it be worth brushing over some resin in the print through areas and flatting back, or am I OK just to go ahead with the clearcoat?