Guys,

This is my 3rd carbon fibre project. It has taken me a great while to complete the mould. Still I am on my learning curve. 

This is the largest mould I have made and it had me up until 0330 last night. I underestimated how long the reinforcement took to lay down and wet through.

I have some areas like in the corners that haven't wetted through. Am I able to add another coat of tooling resin to the whole piece or will it fail to integrate?

Thanks. 

Is it possible to add one more thick layer of reinforcement or will it fail to bond?





Edited 6 Years Ago by ats101
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search