How to solve this wrap carbon problem?
How to solve this wrap carbon problem?
Post Reply
Like
3
How to solve this wrap carbon problem?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
TomDesign
TomDesign
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
why im getting these small bubles? after i lay resin and if i brush soft paper then clean all dusk stay inside... can someone advise what to do? or simply lay first layer epoxy then lay gc50 and to polish without brushing surface not to get dusk into tiny holes.
Edited
13 Years Ago by
TomDesign
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
How to solve this wrap carbon problem?
TomDesign
-
13 Years Ago
[quote][b]TomDesign...
fgayford
-
13 Years Ago
i always waited till it dry and then putted each layer more. and last time i tryed to wait till...
TomDesign
-
13 Years Ago
I did a simillar project with a helmet I skinned with epoxy resin. I've used laminating epoxy (quit...
matthieutje65
-
13 Years Ago
Thanxs Matt what about thing that Warren suggesting simply couple layers epoxy the to spray GC50...
TomDesign
-
13 Years Ago
I have never worked with glass bubbles, neither with GC50 so I can't tell you more about that...
matthieutje65
-
13 Years Ago
i was reading about making your own pre preg CF. the article stated the amount of epoxy needed was...
brasco
-
13 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search