By TomDesign - 12/23/2012 3:57:39 PM



why im getting these small bubles? after i lay resin and if i brush soft paper then clean all dusk stay inside... can someone advise what to do? or simply lay first layer epoxy then lay gc50 and to polish without brushing surface not to get dusk into tiny holes.
By brasco - 12/31/2012 3:52:38 AM

i was reading about making your own pre preg CF. the article stated the amount of epoxy needed was about the same weight of CF
.if you make too much epoxy it will get bubbles in it as you brush it. when we do FG and polyester repairs on heavy trucks when the tires blow and
blast the fenders apart, we take the FG and wet it down in pieces and then lay them in wet on wet till the shape is built up. then use heat lamp or heat gun (in cold shop climates) and warm it up to get the exotherm to kick off.
 with CF the epoxy will puddle as it warms up for its exotherm process and it's viscosity goes to pot. IE it is thick when cool and gets runny as it heats up.
if you have an old air conditioning vac pump( most all AC for automotive applications are done with recycling machines) you could put your resin after mixing in a vessel and vac it down to de gass it. then brush or use bondo spreader to spread the epoxy onto your dry CF.
 for your pre preg. use plastic sheeting to keep sheets separate til you need them. you can make small quantities with air dry epoxy
and it will be ok, just dont make more than you will likely use.
 you can also blend catalyst (if from same maker and same products) to make a custom temperature mix. too much MEKP will cause bubbles in the polyester and i am 99% same for epoxy.