Hi there

i just did a few tests and I have a problem I already had a few days ago without finding the origin.
When demoulding I heard a lot of crrrrrrac (It was extremely difficult to demould) annnnd: 
photos worth more than words: 



As you can see resin sticked on the glass despite the use of chemical release agent so I'm wondering what are the differents possible reasons of this fail.... temperature? too early demoulding? fail when applying the release agent?
something else?

Since I'm here, what's the best way to cut Polypropylene Sheets? I'm thinking about using it instead of glass for the next time.

Thank you mates
Edited 6 Years Ago by GEFF
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search