Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Yeh sort of answered your own question there, could be any of those things. Its a release failure for sure, but without knowing exactly what you did and what you used, its pretty impossible for us to conclude what failed.
For cutting polypropylene, a jigsaw is probably the easiest. It will heat up and melt as you cut it, but the back of a razor blade makes pretty short work of deburring the edge afterwards. Polypropylene is no where near as good a tool surface as glass though, I'd definitely recommend persisting with glass and just getting the release issues sorted.
|