TO82
TO82
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 6,
Visits: 311
After some info on carbon skinning mainly what people use as the 'basecoat' is it possible to use polyester resin or gel coat as the first layer for which the carbon is placed upon?
Also which type of cloth is easier to work with 1x1 or twill weave 2x2?
Thanks for any help!
Cheers
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Skinning queries
TO82
-
13 Years Ago
Bump, Looking to skin some abs plastic door handles, Can it be done using just polyester resin...
TO82
-
13 Years Ago
[quote][b]TO82 (20/12/2012)[/b][hr]Bump, Looking to skin some abs plastic door handles, Can it be...
fgayford
-
13 Years Ago
hello TO82, from what I have seen yes, it is possible to use polyester resin to skin your parts...
WilliamsHPF
-
13 Years Ago
to82 i started since 4 years and till now i had no epoxy clear at my town, i use polyester to...
mhdghoul
-
13 Years Ago
yes i done with polister but after 1 month clear coat start to be pain as polyster tart to move and...
TomDesign
-
13 Years Ago
i come from an automotive repair background(collision repair specifically) and if you clear use fine...
brasco
-
13 Years Ago
Done an overlay with polyester followed by clear coat, doesnt look too bad in dayligt yet when i...
TO82
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search