Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Coulpling coat
Coulpling coat
Post Reply
Like
3
Coulpling coat
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Shaneer22
Shaneer22
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 156,
Visits: 14K
Does any one no the maximum open time is before coupling coat can be applied can the open time be days.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Coulpling coat
Shaneer22
-
13 Years Ago
Hi, assuming you are talking about the Uni-Mould System. I usually apply the coupling coat when the...
wozza
-
13 Years Ago
I usually make my molds from epoxy so the open time is crucial,this is first time using unimo D...
Shaneer22
-
13 Years Ago
I have used 2% Catalyst in the past on the gel coat because at 1% the gel coat was taking too long...
wozza
-
13 Years Ago
I having given it two gel coats first coat catalized at 2% and second gelcoat at 1% because I wasn't...
Shaneer22
-
13 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search