By Shaneer22 - 12/16/2012 6:13:47 PM				
            
                      
            Does any one no the maximum open time is before coupling coat can be applied can the open time be days.
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By Shaneer22 - 12/16/2012 10:44:17 PM				
            
                      
            I having given it two gel coats first coat catalized at 2% and second gelcoat at 1% because I wasn't sure of open time for coupling coat,I think am going to bring part to work and give it coupling coat mid morning then apply main reienforcement about 6 that should be sufficient time.
           
		 | 			
		 
	
	
						
		 	
		
	 |