Tomorrow I will finally infuse the 12' canoe I have been working on for years. I'm going to preheat the mold and I want to elevate the temperature some during the curing process.
What is the ideal temperature I should aim for regarding the mold? The resin I am using has a cps of 600 so I think it needs to thin some once it hits the mold.
I also want to elevate the temperature once the infusion has completed. Is there a limit as to what this temperature can be?
Thanks again for offering such a great resource for those with limited knowledge in this area.
Alan


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
ahender - 6 Years Ago
explorecomposites - 6 Years Ago
ahender - 6 Years Ago
torstenker - 6 Years Ago
ahender - 6 Years Ago
ahender - 6 Years Ago
Hanaldo - 6 Years Ago
explorecomposites - 6 Years Ago
ahender - 6 Years Ago
Hanaldo - 6 Years Ago
ahender - 6 Years Ago
ahender - 6 Years Ago
Warren (Staff) - 6 Years Ago
             Thank you Warren.
ahender - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search