Hello, so I'm working with nomex honeycomb panels with composite fiber on either side. I have a series of screws entering one side of the laminate, but not exiting the other. My question is what composite fiber would be best at retaining the screws (like most resistant to a normal force)? Previously I've been skinning the honeycomb entirely with carbon. But the screw retention feels a bit weak.

The application here is honeycomb cored skis.

A few options:
Fiberglass
Basalt
Kevlar

And I'm guessing these are not the way to go, but perhaps?:
Dyneema
Innegra
Flax

I'd put down carbon, but from past experience it doesn't provide much support to holding screws in the laminate

Thanks!
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
thelongride - 6 Years Ago
Rosta Spicl - 6 Years Ago
SleepingAwake - 6 Years Ago
thelongride - 6 Years Ago
SleepingAwake - 6 Years Ago
thelongride - 6 Years Ago
SleepingAwake - 6 Years Ago
thelongride - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search