As the title states I am looking for feedback on how to make my resin infusion better.  How can I do better?
I noticed I may wan the peel ply to extend further than the infusion mesh for easier removal.

Please provide feedback after viewing my video:

YouTube Video link

After the infusion there were some parts that stuck to the PVA instead of the carbon.



Showing PVA film on mirror surface.