Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Mould Making
»
Female and male mould
Female and male mould
Post Reply
Like
9
Female and male mould
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
kosak95
k
kosak95
posted 6 Years Ago
ANSWER
HOT
Topic Details
k
Group: Forum Members
Posts: 14,
Visits: 518
Hi,
Is it a good idea to make female and male mould for resin infusion of carbon fibers?
I'm making helmet and was interested if it is a good idea?
Thanks
Reply
Like
9
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Female and male mould
kosak95
-
6 Years Ago
are you refering to a mould and countermould so you have a moulded surface on moth sides of your laminate? In this case this will not work well with resin infusion. One solution would be to create a....
SleepingAwake
-
6 Years Ago
Yes I was thinking of mould and counter mould made of rigid material. I already did some helmets with mould and film on the other side and it was okay, not perfect because of pinholes and some...
kosak95
-
6 Years Ago
bridging and porosity are not going to be solved with a counter mould. this probably just comes down to skills and techniques of the laminator and will come with time... What process for serial...
SleepingAwake
-
6 Years Ago
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search