			            Yes I was thinking of mould and counter mould made of rigid material.
 I already did some helmets with mould and film on the other side and it was okay, not perfect because of pinholes and some bridging.
 What do you recommend? silicone or something else to get as good surface as it could be on both sides?
 And additional question, what would be best way to make serial production of helmets made of carbon, with which process?
 
 |