Bottle cap table


Author
Message
mmcqui
m
Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)
Group: Forum Members
Posts: 1, Visits: 12
Hi there

Looking for some advice, poured my resin one week ago on a grouted bottle top table, apart from a couple of small bubbles, I was fairly happy with for a first attempt at resin.

I went to give the table a wipe down last night and on drying it I noticed that there appears to be a film after cleaning, especially on the outer of the table. I’m fairly sure it was ok before cleaning but I am absolutely sure it wasn’t there a couple days ago.

Do I need to sand down and pour again or will polishing help this, I’m pretty gutted as it looked great. It still looks shiny at a distance but under direct light and up close it’s not great.

I have tried to wipe with just water and it clears until dry.

Any help would be appreciated

Matthew
GO