Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - Product Specific Pages
»
Carbon Fibre Tube and Section
»
roll wrapped Carbon fibre tube finish?
roll wrapped Carbon fibre tube finish?
Post Reply
Like
11
roll wrapped Carbon fibre tube finish?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Matt (Staff)
Matt (Staff)
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 680,
Visits: 1.9K
Is there a plan in the company to supply 14/15mm as well?
In pultrusion, probably not. In our experience, generally, once the required diameter is up much beyond 12mm (with exception of the aforementioned fishing poles!) the loads on the tube tend to be less unilateral and therefore it gets harder to successfully use unidirectional pultrusions and more appropriate to use roll wrapped tubes. This is why we have the 'handover' between pultrusions and roll-wrapped tubes around the 10/12mm mark.
All the best, Matt
Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Reply
Like
11
wozza
wozza
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
Hi, sorry if my suggestion about the Rods/Poles was incorrect but the ones in my local shop are roll wrapped. I spoke with the shop owner today and it turns out the Rods/Poles I have seen there are made by a local chap specifically for him and not commercially available.
Regards Warren
Carbon
Copies Ltd
Reply
Like
9
dyobyrag
dyobyrag
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 4,
Visits: 8
Hey lads,
First off, Kev:
I did indeed read the product description, but
"
The phrase ‘roll wrapped’...
(this is what gives roll-wrapped tubes their characteristic ribbed appearance)
"...
but in my experience, a product may appear ribbed but be in fact have a smooth finished and vice-versa.
I would have to agree with Matt on the fishing rod. Now im no fishing expert but Ive only ever seen them in a pultrusion form and being smooth.
Thanks Matt, thats clears that up then. Also I noticed that your pultruded tubes only go up to 12mm. Is there a plan in the company to supply 14/15mm as well?
Thanks to everyone for adding their opinions and helping out.
G
Reply
Like
10
Matt (Staff)
Matt (Staff)
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 680,
Visits: 1.9K
Hi G,
The way to describe it would be ribbed rather than rippled. The 'steps' on the surface are simply a function of the shirnk tape that's spiral round around them during the manufacturing process. I think the photos on the website give an acurate idea of what the tubes look like. If you slide your nails over the surface you'll hear a slight 'zzzzz' sound as they go over the faint ribs.
When Warren says that you'll find this finish on fishing poles, this certainly won't
always
be the case. I'm not a fisherman but so far, of the poles I've seen customers bring in to ask about how to repair them, I've only ever seen carbon fibre tubes that have been manufactured by pulltrusion, they therefore have a smooth finish from the
pultrusion process
.
All the best, Matt
Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Tags
carbon fibre
finish
pultrusion
roll wrapped
unidirectional
Reply
Like
11
wozza
wozza
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
As explained above it does have a slight "ribbed" surface. Depending on where you are in the world? if you want to see it for real pop into your local fishing tackle shop and have a look at the Carbon Rods/Poles most are produced using the Roll Wrap technique.
Regards Warren
Carbon
Copies Ltd
Reply
Like
9
Kevin-Lee
Kevin-Lee
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 44,
Visits: 2.4K
Hi,
Quoted from the EC product page...
"
The phrase ‘roll wrapped’ refers to the process used to manufacture these tubes. The pre-preg carbon fibre is first laid up around a mandrel in multiple layers. Once the reinforcement is in place it is spiral wrapped with heat-shrink tape (this is what gives roll-wrapped tubes their characteristic ribbed appearance) before the whole assembly is oven cured."
Kev.
Reply
Like
11
dyobyrag
dyobyrag
posted 14 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 4,
Visits: 8
Hello,
Just a quick question. The rolled wrapped carbon fibre tubing, is there a smooth finish on it or is it kind of rippled?
Thanks
G
Tags
rolled wrapped carbon fibre finish?
Reply
Like
11
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
11
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search