Pva application fish eyeing


Author
Message
moonpie
moonpie
Supreme Being (444 reputation)Supreme Being (444 reputation)Supreme Being (444 reputation)Supreme Being (444 reputation)Supreme Being (444 reputation)Supreme Being (444 reputation)Supreme Being (444 reputation)Supreme Being (444 reputation)Supreme Being (444 reputation)
Group: Forum Members
Posts: 34, Visits: 94
I have a big plug I'm ready to mould. After so many failures with easy lease I was going to use pva.  The plug is sealed with s120 and has a clean smooth finish. When I apply pva though it fisheyes like its a wax resist crayon picture and I get bad patchy coverage.  Is there something anyone can recommend to prepare the surface for pva application?  I always pre clean with EC mould cleaner so it should be contaminant free...thanks
Edited 6 Years Ago by moonpie
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
moonpie - 6 Years Ago
beliblisk - 6 Years Ago
moonpie - 6 Years Ago
Hanaldo - 6 Years Ago
moonpie - 6 Years Ago
LibertyMKiii - 6 Years Ago
Hanaldo - 6 Years Ago
moonpie - 6 Years Ago
ats101 - 6 Years Ago
beliblisk - 6 Years Ago
moonpie - 6 Years Ago