		| By moonpie - 6/26/2020 8:16:17 PM 
 I have a big plug I'm ready to mould. After so many failures with easy lease I was going to use pva.  The plug is sealed with s120 and has a clean smooth finish. When I apply pva though it fisheyes like its a wax resist crayon picture and I get bad patchy coverage.  Is there something anyone can recommend to prepare the surface for pva application?  I always pre clean with EC mould cleaner so it should be contaminant free...thanks
 |  
		| By moonpie - 9/1/2020 7:22:49 PM 
 Thanks guys, the recent hot weather has allowed me to make the gelcoat touch up outside quite nicely so im on with the sanding now. Once done I need to make two mould flanges as this piece will be made in two halves and bonded together.  Appreciate the advice, thank you! 😉
 |  |