Hi,

I am using glasscast 50 with 2 or 3 colours, base colour will be metallic blue, I would like to know what is the best way of adding a swirl effect in different colours that maintain there shape and don’t bleed in to the blue.

Do I mix all the colours at the same time, pour the base colour wait for it to cure a bit, and the use the other colours if so how long approx do I have to wait for the resin to cure to correct viscosity,

Or can I wait till the resin hits a certain temperature, if so what is that temperature please

Thanks