mscomposites
m
mscomposites
posted 6 Years Ago
ANSWER
HOT
Topic Details
m
Group: Forum Members
Posts: 23,
Visits: 108
Curious if there’s any advantage to leave the part under vacuum overnight and start flowing resin in the morning, or just let it sit under vacuum for an hour or two, make sure no leaks and then pump.
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
De-bulking before infusion
mscomposites
-
6 Years Ago
Unless you are using badly stored aramid, wich is very hydrophilic, there is no advantage of letting the vacuum on your system for a long time. You can dry hydrophilic fibres if you let them at aroun...
oekmont
-
6 Years Ago
Ok cool, yah I wasn’t under the impression that you gained a better overall part from that, just trying to see what other people out are saying about this topic. Thanks for the reply.
mscomposites
-
6 Years Ago
For small stuff you'll probably be fine if you just get the bag down and wait an hour or so (or 20 minutes) and then shoot your infusion. For larger or thicker items or those with cores, or material....
explorecomposites
-
6 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search