Legoman
Legoman
posted 6 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 29,
Visits: 622
Dear EasyComposite!
How is the SMC Vacuum Regulator exactly working?
Reply
Like
8
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
SMC Vacuum Regulator
Legoman
-
6 Years Ago
In essence it allows a very small leak through from air to the bag side of the regulator while minimising leak through on the vacuum side. The design is such that the leak through on the vacuum pump....
Warren (Staff)
-
6 Years Ago
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search