By Legoman - 6/20/2020 7:05:32 PM
Dear EasyComposite!
How is the SMC Vacuum Regulator exactly working?
|
By Warren (Staff) - 6/22/2020 1:25:30 PM
In essence it allows a very small leak through from air to the bag side of the regulator while minimising leak through on the vacuum side. The design is such that the leak through on the vacuum pump side is only around 0.6L/min of air.
|
|