Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
If it is smooth glossy polypropylene then epoxy resin will not stick to it, so demoulding should be quite easy.
I suspect you would want more than 1 layer of cloth - a typical 210gsm cloth is around 4 layers per mm thickness.
If you follow our skinning video - in essence the resin build up process is the same, you would hit it with 3 coats then sand it flat.
Lacquer or polish is personal preference. In very sunny or hot climates, a lacquer will offer more UV stability.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|