PX90 Enigne mounts


Author
Message
Massimiliano
M
Supreme Being (2.3K reputation)Supreme Being (2.3K reputation)Supreme Being (2.3K reputation)Supreme Being (2.3K reputation)Supreme Being (2.3K reputation)Supreme Being (2.3K reputation)Supreme Being (2.3K reputation)Supreme Being (2.3K reputation)Supreme Being (2.3K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Hanaldo - 5/25/2020 2:40:08 AM
You need a special primer to get a very good bond to metal.

Hi Hanaldo,.which one do you recommend?

Hanaldo
Hanaldo
Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
You need a special primer to get a very good bond to metal.
Darren
Darren
Supreme Being (628 reputation)Supreme Being (628 reputation)Supreme Being (628 reputation)Supreme Being (628 reputation)Supreme Being (628 reputation)Supreme Being (628 reputation)Supreme Being (628 reputation)Supreme Being (628 reputation)Supreme Being (628 reputation)
Group: Forum Members
Posts: 54, Visits: 916
Attemping to make some enigne mounts, but not having much luck with urethane bonding to the metal. Previously used Polytek PT flex, which didnt bond.
Does PX90 bond to metal very well? 
Or would it best to cast slightly oversized bushes and press them in?