By Darren
-
5/24/2020 4:44:54 PM
Attemping to make some enigne mounts, but not having much luck with urethane bonding to the metal. Previously used Polytek PT flex, which didnt bond.
Does PX90 bond to metal very well?
Or would it best to cast slightly oversized bushes and press them in?
By mporta71
-
5/25/2020 4:38:46 AM
+
x
Hanaldo - 5/25/2020 2:40:08 AM
You need a special primer to get a very good bond to metal.
Hi Hanaldo,.which one do you recommend?