Carbon Fiber driveshaft


Author
Message
k.alan.bates
k
Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)
Group: Forum Members
Posts: 36, Visits: 664
Would the rules for making a carbon fiber driveshaft follow the normal tube making process detailed in the videos or would there be additional engineering concerns that would change the process?

...I'm just curious. I don't have a large enough oven right now to pull one off anyway (need a 51" ds) ...but it would be neat to make one if it was as simple as making a 4" cf tube.

Thanks.

[Edit: oh, I guess it would be important to point out that yes, it makes perfect sense you would have to align the cloth to provide torsional rigidity and that wasn't a concern in the basic tube making tutorial. I was purposely trying to just throw the open question out to see what kinds of thought processes people might use. But I thought that might be something worth coming back to start the list of differences with.]
Edited 6 Years Ago by k.alan.bates