Hi,
In fist sorry for my poor english.
I made new parts in twill carbon/kevlar, I do not have problem for cut it with electric scissor but after made parts and resin cure I can't cut parts well kevlar make pilling, I have try a lot of things without success, how to have a nice cut without pilling ?

Thanks for your help !
Your youtube video are really nice I love to see it.

Matt