By Matthieu Renard - 5/17/2020 2:56:46 PM
Hi, In fist sorry for my poor english. I made new parts in twill carbon/kevlar, I do not have problem for cut it with electric scissor but after made parts and resin cure I can't cut parts well kevlar make pilling, I have try a lot of things without success, how to have a nice cut without pilling ?
Thanks for your help ! Your youtube video are really nice I love to see it.
Matt
|
By Warren (Staff) - 5/18/2020 4:14:14 PM
You will almost always get some of the kevlar fluff on the edges, even with sanding. However, using a sharp stanley blade/scalpel blade you can trim it off leaving a nice smooth edge.
|
|