carbon man
posted 6 Years Ago
ANSWER
HOT
Topic Details
Group: Awaiting Activation
Posts: 86,
Visits: 1.2K
Sorry tried the search. I while back I seem to remember some one using a alternative. As all spray glue iv tried leaves marks in the Finnished part.
For putting in the mould to help put carbon in place before layup.
like mixing neat resin and acetone and spraying a mist into the mould? (could be completely wrong here)
Thanks
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Spray glue alternative
carbon man
-
6 Years Ago
what spray adhesive did you use? when i need a perfect finish out of the mould i use tha isotacker from sicomin which doesn't leave any traces at all as long as you don't overdo it. I am sure others....
SleepingAwake
-
6 Years Ago
I switched to cheap 2k clearcoat. With the right setup it is really just a thin mist wich gives just the right tackiness. With a clear gelcoat it is absolutely undetectable, even if you sprayed a...
oekmont
-
6 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search