Glasscast 50 Lake table bubble cluster in middle


Author
Message
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
As long as you are careful to keep the hole clean and give it a good sand for adhesion then you should be able to blend the repair in. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Graham
G
Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)
Group: Forum Members
Posts: 2, Visits: 24
I have an annoying cluster of bubbles in the middle of a 12inch diameter resin lake that I could remove with a plunge router, maybe 15-20 mm deep, 50mm diameter. Could I top up with more gc50 and no one would ever know?