I have an annoying cluster of bubbles in the middle of a 12inch diameter resin lake that I could remove with a plunge router, maybe 15-20 mm deep, 50mm diameter. Could I top up with more gc50 and no one would ever know?
|
By Warren (Staff) - 5/7/2020 10:12:07 AM
As long as you are careful to keep the hole clean and give it a good sand for adhesion then you should be able to blend the repair in.
|
|