Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
C SRIKRISHNA - - 4/15/2020 3:36:12 PM
What are composite core facesheets?

Well, I guess 'face sheets' could be a way of describing the skins of laminate either side of the core. So, a foam cored carbon fibre panel for example has skins of carbon fibre laminate either side of a foam core. These skins could also be described as the face sheets.


Matt Statham
Easy Composites / Carbon Mods - Technical Sales
C SRIKRISHNA -
C SRIKRISHNA -
Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)
Group: Forum Members
Posts: 1, Visits: 4
What are composite core facesheets?