Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Sandwich Core
Sandwich Core
Post Reply
Like
3
Sandwich Core
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
C SRIKRISHNA -
C SRIKRISHNA -
posted 5 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 4
What are composite core facesheets?
Reply
Like
3
Matt (Staff)
Matt (Staff)
posted 5 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 680,
Visits: 1.9K
+
x
C SRIKRISHNA - - 4/15/2020 3:36:12 PM
What are composite core facesheets?
Well, I guess 'face sheets' could be a way of describing the skins of laminate either side of the core. So, a
foam cored carbon fibre panel
for example has skins of carbon fibre laminate either side of a foam core. These skins could also be described as the face sheets.
Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search