Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Making my own curved plywood/veneer with vacuum bagging
Making my own curved plywood/veneer with vacuum bagging
Post Reply
Like
2
Making my own curved plywood/veneer with vacuum bagging
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Chris Rogers
C
Chris Rogers
posted 6 Years Ago
ANSWER
HOT
Post Details
C
Group: Forum Members
Posts: 120,
Visits: 933
If you're not making a huge number, vacuum bagging would be easier than making a press. Many ski and skateboard builders use shaped platens on large presses with either hydraulic or pneumatic (like inflated fire hose) clamps. If you can make a simple curved form that holds vacuum then it will work fine. You could make the shape from wood and glue a sheet of plastic or thin aluminum to make the air-tight surface.
Here are two of my articles that might help:
(...could copy and paste but that would be a long post!)
Vacuum Bagging:
https://explorecomposites.com/articles/lamination/basics-vacuum-bagging/
Buying a Vacuum Pump:
https://explorecomposites.com/articles/tools-and-equipment/buying-a-vacuum-pump/
You probably don't need a high vacuum for this so a dry rotary vane, diaphragm or other cheap oil-free pump would be fine. You won't regret having a nice one though if you plan to get into more composite work - just make sure you get a catch-pot too to protect it.
Reply
Like
3
Antoine
Antoine
posted 6 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 12
Hello guys,
I'm a wooden surfboard builder and I have the project to build some kitesurf boards like on the following pictures:
I'm not sure about which technique to use to glue those sheets of wood together with a curve and even some concaves (like a skateboard).
I have no experience at all in vacuum bagging but I thought of using a mold and vacuum bagging technique to glue them together. My questions are:
- Could you light me on the technique to use, or maybe send me a link to a tutorial for similar results.
- I'm thinking of buying the starters set with the vacuum pump? Would that be sufficient or do would I need extra material (I plan to glue either with PU glue or with epoxy)
Thank you so much for your help and greets from Portugal,
Antoine
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search