Group: Forum Members
Posts: 338,
Visits: 2K
|
With regard to the GC50 in-mould coating...it is very much like a polyester gel coating, so scratches and scuffs can be flatted and polished back up again. Anything deeper can be filled with a little epoxy resin and also flatted and polished. As long as you don't go too deep with the flatting work, it is a very good surface on which to carry out repairs
|